Group: Administrators
Posts: 167,
Visits: 4.6K
|
Colder temperatures can have a significant effect on the viscosity of the resin - thicker resin is more difficult to mix which in turn can mean more air is entrapped whilst mixing but more importantly in this situation has the potential to make air release much more difficult to achieve.
Do you use a hot air gun/blow torch over the surface at all and do you know a) what temperature the resin/hardener is being stored and and b) what temperature you're working in?
|