Hi there,
I am trying to make the attached part in carbon by resin infusion. I did some experiments which went not so bad, but I am not yet sure how to split the mould (actually I splitted in the middle) to have a good look for the front curve.

My other problem is that the part is pretty thin when I use infusion and it is very difficult to match the upper and lower part on this small base. Has anyone a good idea what I can do to make brighter edges? soric?

And how do you glue the two parts together to have a fine line and a good gloss?

Thanks a lot Wink
SHaas
S
Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)
Group: Forum Members
Posts: 46, Visits: 383
SHaas - 1/3/2018 6:12:36 PM
Hi there, I am trying to make the attached part in carbon by resin infusion. I did some experiments which went not so bad, but I am not yet sure how to split the mould (actually I splitted in the middle) to have a good look for the front curve. My other problem is that the part is pretty thin when I use infusion and it is very difficult to match the upper and lower part on this small base. Has anyone a good idea what I can do to make brighter edges? soric?And how do you glue the two parts together to have a fine line and a good gloss?Thanks a lot Wink
so here are the pictures. perhaps I should wrap a soric in carbon reinforcements an make the infusion?