Hi there,
I am trying to make the attached part in carbon by resin infusion. I did some experiments which went not so bad, but I am not yet sure how to split the mould (actually I splitted in the middle) to have a good look for the front curve.

My other problem is that the part is pretty thin when I use infusion and it is very difficult to match the upper and lower part on this small base. Has anyone a good idea what I can do to make brighter edges? soric?

And how do you glue the two parts together to have a fine line and a good gloss?

Thanks a lot Wink
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search