Hi,
Is it possible to postpone the post-curing cycle?
I mean build the mould and let it cure at ambient temperature then perform the post-cure cycle  after 2 months when my oven is available?

What would be a correct post-cure temperature for a carbon glider that will be exposed to extensive sun heat during summer?
I am thinking 100C for moulds and 75 for parts?

Thanks for your support
Olivier
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
When you say glider, do you mean like a RC glider or an actual full-size sailplane?

If it's the latter, I would not recommend doing exposed carbon. It isn't actually allowed here in Australia, and for good reason - in full sun you will see excessively high temperatures. You would need a pre-preg cured above 150C for it to be stable. 