Group: Forum Members
Posts: 26,
Visits: 89
|
Hi, Is it possible to postpone the post-curing cycle? I mean build the mould and let it cure at ambient temperature then perform the post-cure cycle after 2 months when my oven is available?
What would be a correct post-cure temperature for a carbon glider that will be exposed to extensive sun heat during summer? I am thinking 100C for moulds and 75 for parts?