By Olivier - 11/25/2017 7:22:03 PM
Hi, Is it possible to postpone the post-curing cycle? I mean build the mould and let it cure at ambient temperature then perform the post-cure cycle after 2 months when my oven is available?
What would be a correct post-cure temperature for a carbon glider that will be exposed to extensive sun heat during summer? I am thinking 100C for moulds and 75 for parts?
Thanks for your support Olivier
|
By Hanaldo - 11/27/2017 12:51:54 PM
When you say glider, do you mean like a RC glider or an actual full-size sailplane?
If it's the latter, I would not recommend doing exposed carbon. It isn't actually allowed here in Australia, and for good reason - in full sun you will see excessively high temperatures. You would need a pre-preg cured above 150C for it to be stable.
|
|