Vinz
Vinz
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 57
Hello,
Now, I am using Durepox Clear coat, and I need 3 layers at least to have good results.
I would like to decrease the number of layers, and I would like to know your experiences with different clearcoats.
Does someone know a high hiding clearcoat?
Vinz
Vinz
www.carbonara-tech.ch
Reply
Like
2
Reply
Vinz
Vinz
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 57
I've tried Basco clear coat, and it's very nice! Perfect finish!
Vinz
www.carbonara-tech.ch
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Clear coat choice
Vinz
-
9 Years Ago
for little parts I use 2k clear coat in rattle can, usually 1 or 2 layers gives me good result (depending on the quality surface). For bigger parts I ask to a professional car painter that use high.....
Saff
-
9 Years Ago
+ x [quote] [b] Saff - 10/19/2017 9:50:56 AM [/b] + x [quote] [b] Vinz...
Interloper393
-
9 Years Ago
Any 2k clearcoat will be fine. I use max meyer 0300.. perfect parts and gloss every time
Interloper393
-
9 Years Ago
If I want a real deep finish, I use basco lacquer. They also got clear filler, wich works brilliantly. But I am certainly no painting expert. Usually I'll leave this to a painter.
oekmont
-
9 Years Ago
Hello I use MIPA CC9 High Solid Clear Coat. 2 layers prefect surface!
Jaspen
-
9 Years Ago
I've tried Basco clear coat, and it's very nice! Perfect finish!
Vinz
-
9 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search