Hello,

Now, I am using Durepox Clear coat, and I need 3 layers at least to have good results.
I would like to decrease the number of layers, and I would like to know your experiences with different clearcoats.
Does someone know a high hiding clearcoat?

Vinz

Vinz
Reply
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
Any 2k clearcoat will be fine. I use max meyer 0300.. perfect parts and gloss every time