Hi,
I have a pattern of a rc glider stabiliser made of foam and several layers of IN2, pattern coat primer and pattern coat hi gloss. I am making an epoxy mould with this pattern and EG60 + FG layers + IN2 + poraver.
I need to know if I should post cure the pattern before making the mould and what is the Tg of pattern coat primer and hi gloss Or build the mould and post cure it? Should I post cure the mould with or without the pattern? I plan to perform a post cure cycle as noted in TDS: :• 24 hours at 25°C• 2 hours at 40°C• 2 hours at 50°C• 2 hours at 60°C
Do I get the same properties if I wait 15 days and no post cure? For the final CF stabiliser can I post cure the part up to 60C?
Thanks for your support
Kind Regards, Olivier
|