Post curing of mould made of EG60 epoxy tooling gelcoat


Author
Message
Olivier
Olivier
Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)
Group: Forum Members
Posts: 26, Visits: 89
Hi,

I have a pattern of a rc glider stabiliser made of foam and several layers of IN2, pattern coat primer and pattern coat hi gloss.
I am making an epoxy mould with this pattern and EG60 + FG layers + IN2 + poraver.


I need to know if I should post cure the pattern before making the mould and what is the Tg of pattern coat primer and hi gloss
Or build the mould and post cure it?
Should I post cure the mould with or without the pattern?
I plan to perform a post cure cycle as noted in TDS: :• 24 hours at 25°C• 2 hours at 40°C• 2 hours at 50°C• 2 hours at 60°C

Do I get the same properties if I wait 15 days and no post cure?
For the final CF stabiliser can I post cure the part up to 60C?

Thanks for your support

Kind Regards,
Olivier


Reply
Olivier
Olivier
Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)Supreme Being (140 reputation)
Group: Forum Members
Posts: 26, Visits: 89
Warren (Staff) - 11/16/2017 9:14:41 AM
As you are mostly using IN2. you can post cure the pattern using the IN2 post cure from the TDS.

In essence you can then allow the mould to cure for 24 hours before following the post cure cycle with the pattern still in the mould.

In reality, with the low temperatures and relatively slow 10C steps, It is unllikely you would have any distortion or sagging from the mould softening and likewise there are unlikely to be any CTE issues between the slightly different materials, so in practice you could do it either way without any issues.

Thanks Warren,
Could you give me the HDT of Pattern coat primer please?