How to proceed with infusion, tricky mould


Author
Message
Ville
V
Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)
Group: Forum Members
Posts: 2, Visits: 28
Hello

Newbie here

I did two infusions with this mould made with the starter kit, totally failed



The boxed shape corners were not completely pressed in by vacuum, I should have known that. Had too much epoxy in the corners and dry points..
I did try infu-tac, but gave up on it because I mainly messed up and and tore the fabric, messy stuff.. Should I glue the center first and move towards the corners with the glue, or glue in corners only?


Then should I get gelcoat along with infu-tac, as it would leave a cloudy finish? Should I use it post-production or spray in the mold, and does it then work like glue?
Or making my own epoxy tack spray. But am I likely to mess it up? 100:5 epoxy/hardener maybe

So many questions, more to come.

This a good setup for infusion? I used compoflex. Would normal infusion mesh and peel ply be better?



And I had troubles not getting a perfect vacuum. I could not find any leaks but air was getting in from somewhere. There is some damage on the mould caused by removing the pattern, and sanding too much. Think I need to check that the mould is not leaking too.

How should I proceed next time with the infusion. Carefully cutting the fabric in the corners and using glue with other layers also?

Thanks in advance
Ville

edit: pics in google photos, photobucket sucks
https://photos.app.goo.gl/IwY2Fai8QMmB4FV13
Edited 8 Years Ago by Ville
Reply
Ville
V
Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)
Group: Forum Members
Posts: 2, Visits: 28
Thanks. I wonder why I was planning on using only a single piece, cutting separate pieces each side sounds a lot easier. And it will do a better job with my skills.

I have a roller and ec-cutter available. I'll try spray-tack before cutting. Top tip.

And I'll test if the mould holds vacuum with just bagging film, and no pleats. I'm looking to make a few pieces. It will be a batterybox for an ebike, eventually.

I got one part nicely out of the mould. But it was so bad I didn't take pictures of it yet, hehe.