Depending on the surface treatment of the wooden oar, you may only need to apply a good number of layers of release wax. Certainly if the wooden oar is varnished/laquered with a high Gloss then 5- 7 coats of release wax maybe all you need :-) If the oar is scratched, dinged and has a very worn surface, you may need to sort this out, any "open" wood will need to be sealed or laquered, preferably using epoxy coating or 2-component laquer