Warren (Staff) (28/03/2017)
In terms of coating the surface with a fresh layer of resin?  Yes certainly.  It can be a good way of both restoring a damaged boat hull at the same time as making it tidy enough to take a mould from.


Excellent! And it would bond to Polyethylene? 
Lino Blanco Pereira
Lino Blanco Pereira
Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)Forum Member (37 reputation)
Group: Forum Members
Posts: 3, Visits: 37
Hi Matt

I have a question. Im learning to use 3D prínting, because I want use it to Pattern Coat make, can I Apply Primer pattern Coat in 3D parts made in Strength PLA Ingeo HR3D870 filaments (120 Celsius )? Or I must Apply XCR before?

Regards
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search