ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 20
I am currently producing a plug to produce a fairly large multipiece mould for a model boat hull.The plug is an existing ABS plastic vac formed hull that has had alterations/additions in wood and bumper filler.The hull has been strengthened inside to increase rigidity to the necessary level.
My principle question is,can I safely use the pattern coat system over the top of this to get the desired finish?
I know I am safe with wood and the polyester based filler,but is the pattern coat system safe to use on Rigid ABS plastic?I do intend on using no finer than 120 grit prior to application in order to get a decent key.
Kind Regards
Nigel
Reply
Like
26
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Pattern coat system on ABS plastic
NMBROOK
-
10 Years Ago
ABS and styrene generally don't play nicely together - you'll have a big mess on your hands. You...
Hanaldo
-
10 Years Ago
Thank you Hanaldo This does tie in with what I have read regarding polyester resins and ABS on...
NMBROOK
-
10 Years Ago
Sort of depends on the epoxy you can get. If you can get EC's XCR coating resin, then I would say...
Hanaldo
-
10 Years Ago
Hi Nigel, I would agree that you should well be able to skip a step by not using the pattern coat...
Matt (Staff)
-
10 Years Ago
Hi MattI have a question. Im learning to use 3D prínting, because I want use it to Pattern Coat make, can I Apply Primer pattern Coat in 3D parts made in Strength PLA Ingeo HR3D870 filaments (120...
lino80
-
9 Years Ago
Thank you very much Hanaldo and Matt I have already been looking at the XCR resin,I also have a...
NMBROOK
-
10 Years Ago
Hi Nigel, Yes, you can definitely add pigment to aid with sanding. All you need to do is ensure the...
Warren (Staff)
-
10 Years Ago
Thanks Warren That's the route I will go down :) Kind Regards Nigel
NMBROOK
-
10 Years Ago
Could this idea be used on a partly worn kayak hull to give a fresh smoother finish before making a...
Junior
-
9 Years Ago
In terms of coating the surface with a fresh layer of resin? Yes certainly. It can be a good way of...
Warren (Staff)
-
9 Years Ago
[quote][b]Warren (Staff) (28/03/2017)[/b][hr]In terms of coating the surface with a fresh layer of...
Junior
-
9 Years Ago
Post Reply
Like
26
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search