Group: Forum Members
Posts: 3,
Visits: 18
|
Thank you so much for your reply. when it comes to making the mask itself in the silicone mould, I will be using a lay up technique with fiberglass and resin. My geltop coat has wax in to make it glossy. I am wondering what release agent would work between the silicone mould and the gelcoat of the mask. I was thinking of using the Cil release as it gave good release results between the mould and the jacket mould but would that leave residue or damage the top layer of the mask? I am hoping for a super glossy finish.
|