Hello.  So I am looking to make a part for my watercraft. The part has two parts.  Essentially a top and bottom (bottom piece would add a structure or rigidity to the part).  Questions.

Is my best bet to somehow (I am just spit balling here) add a "skeleton" structure between a bottom and top layer of carbon fiber OR should I build the two separate and "combine"?

If I combine two parts, how do I do that?  Do I infuse top part, bottom part and THEN do another infusion with pieces together?  Is that possible?

If not what is the best way to combine two parts? (example you have a cured part a and part b)

Thanks for all your help.  If I am talking crazy its the inexperience talking.
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
3Dersa - 8/18/2017 3:01:47 PM

Gracias por su respuesta, en cuanto a la resina, indican que esta resina se utiliza para hacer llaveros con fotografías dentro y otras opciones de múltiples productos, referencia adjunta. Los componentes de la resina son bisfenol A y epiclorhidrina, del endurecedor Monophenol B y polioxipropilendinamita. Compré productos EasyComposite y no quiero perderlos usando una resina mala. Gracias por adelantado.

Translates as :
Thank you for your response, regarding the resin, indicate that this resin is used to make keyrings with photographs inside and other options of multiple products, attached reference. The components of the resin are bisphenol A and epichlorohydrin, the hardener Monophenol B and polyoxypropylendinamita. I bought EasyComposite products and I do not want to lose them using a bad resin. Thanks in advance.


Looking at the ingredients they are just standard components found in many a "bisphenol A" based epoxy so does not reveal much about the resins properties.

The picture shows a  typical application for a clear casting epoxy.  If that is the kind of project you are trying to do then i would recommend our  GlassCast Clear Epoxy Surface Resin as it can be poured in layers up to 15mm thick and deeper with multiple pours. Quite a few of our customers have used it with "waney edged" wood projects.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
3Dersa
3Dersa
Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)Forum Member (25 reputation)
Group: Forum Members
Posts: 4, Visits: 127
[Citar]
SegundoWarren (personal) - 18/8/2017 3:22:57 PM[/ Segundo]
[Citar]
Segundo3Dersa - 8/18/2017 3:01:47 PM[/ Segundo]

Gracias por su respuesta, en el momento de la resina, la indicación de que esta se utiliza para hacer llaveros con fotografías y otras opciones de múltiples productos, referencia adjunta. Los componentes de la resina son bisfenol A y epiclorhidrina, del endurecedor Monofenol B y polioxipropilendinamita. Compré productos EasyComposite y no quiero perderlos usando una resina mala. Gracias por adelantado.

Traduce como:
Gracias por su respuesta, en cuanto a la resina, indican que esta resina se utiliza para hacer llaveros con fotografías dentro y otras opciones de múltiples productos, referencia adjunta. Los componentes de la resina son bisfenol A y epiclorhidrina, el endurecedor Monofenol B y polioxipropilendinamita. Compré productos EasyComposite y no quiero perderlos usando una resina mala. Gracias por adelantado.

[/ Citar]

Mirando los ingredientes que sólo los componentes estándar se encuentran en muchos un "bisfenol A" basada en epoxi por lo que no revela mucho sobre las propiedades de las resinas.

La imagen muestra una aplicación típica para un epóxido de colada transparente. Si ese es el tipo de proyecto que está tratando de hacer, nuestro nuestro recomienda nuestro  GlassCast Clear Epoxy Resina de superficie, ya que puede puede verter en capas de hasta 15 milímetros de espesor y más profundo con virgen de múltiples. Muy pocos de nuestros clientes han sido utilizados con proyectos de madera "waney bordeados".
[/ Citar]

Ok, pero necesito usar con fibra de carbono Twill no  madera. Your product Resin A and B can not buy it by airmail.

Edited 8 Years Ago by 3Dersa
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
40FordPU - 8 Years Ago
Hanaldo - 8 Years Ago
40FordPU - 8 Years Ago
Hanaldo - 8 Years Ago
3Dersa - 8 Years Ago
Warren (Staff) - 8 Years Ago
3Dersa - 8 Years Ago
Warren (Staff) - 8 Years Ago
3Dersa - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search