Combining two parts


Author
Message
40FordPU
40FordPU
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 3, Visits: 6
Hello.  So I am looking to make a part for my watercraft. The part has two parts.  Essentially a top and bottom (bottom piece would add a structure or rigidity to the part).  Questions.

Is my best bet to somehow (I am just spit balling here) add a "skeleton" structure between a bottom and top layer of carbon fiber OR should I build the two separate and "combine"?

If I combine two parts, how do I do that?  Do I infuse top part, bottom part and THEN do another infusion with pieces together?  Is that possible?

If not what is the best way to combine two parts? (example you have a cured part a and part b)

Thanks for all your help.  If I am talking crazy its the inexperience talking.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
40FordPU - 9 Years Ago
Hanaldo - 9 Years Ago
40FordPU - 9 Years Ago
Hanaldo - 9 Years Ago
3Dersa - 9 Years Ago
Warren (Staff) - 9 Years Ago
3Dersa - 9 Years Ago
Warren (Staff) - 9 Years Ago
3Dersa - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search