Coxo
Coxo
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 39,
Visits: 476
Hi can any help what's the best way to cut the 245
With out it fraing as it's to make a join
Reply
Like
9
scottracing
scottracing
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
put masking tape on the edges and use a pizza cutter or really good shears
Reply
Like
10
Coxo
Coxo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 39,
Visits: 476
But when I peel the tape off will.
It not mess the weave up
Reply
Like
8
Interloper393
Interloper393
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 90,
Visits: 634
Spray glue the back, let it dry and you should be able to cut it perfect
Reply
Like
9
MarkMK
MarkMK
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 338,
Visits: 2K
As mentioned above, some spray tack misted over the cut line. An Olfa roller cutter is also very useful for making clean cuts
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search