Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
Hand Layup
Cutting 245 g carbon
http://www.talkcomposites.com/Topic23684.aspx
By Coxo
-
7/19/2017 11:55:42 AM
Hi can any help what's the best way to cut the 245
With out it fraing as it's to make a join
By MarkMK
-
7/31/2017 11:09:50 AM
As mentioned above, some spray tack misted over the cut line. An Olfa roller cutter is also very useful for making clean cuts