Dezer
Dezer
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 74,
Visits: 1.8K
Hi Guys,
I have a problem in my vacuum infusion process, with the vacuum pump turned on the pressure is constantly at 0.9 atm, but if I turn off the vacuum line the pressure starts to drop. I have already looked for microwaves and can not find anything.
Is it a problem for me to infuse the part and keep the pump running constantly until the healing time?
Tags
leakage
pressure vacuum
resin infusion
vacuum infusion
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Leakage when shutting off the vacuum pump
Dezer
-
9 Years Ago
Are you clamping the exit line also, as it's not uncommon to find that the leak is from your catch...
MarkMK
-
9 Years Ago
It can also be the pump itself. Without any mechanism to hold vacuum I have seen some pumps run backwards for a bit when turned off. I have a one way valve right on the pump.
Fasta
-
9 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search