Hi friends, 

I would like to make a tube in the vacuum infusion process, but it has a complex shape, some tips or techniques how to do it?

Example:

http://www.talkcomposites.com/Uploads/Images/0cd945f3-a3c5-43a5-b9a9-916d.jpg

Grateful for everyone's attention!! 
Reply
Dezer
Dezer
Supreme Being (984 reputation)Supreme Being (984 reputation)Supreme Being (984 reputation)Supreme Being (984 reputation)Supreme Being (984 reputation)Supreme Being (984 reputation)Supreme Being (984 reputation)Supreme Being (984 reputation)Supreme Being (984 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
I don't have any autoclave, it makes my job with prepreg difficult, and the cost of the part would be more expensive as well.

matthieutje65, thanks for your help.