Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Tubes with complex shapes
Tubes with complex shapes
Post Reply
Like
8
Tubes with complex shapes
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Dezer
Dezer
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 74,
Visits: 1.8K
Hi friends,
I would like to make a tube in the vacuum infusion process, but it has a complex shape, some tips or techniques how to do it?
Example:
Grateful for everyone's attention!!
Tags
pipes
tips
tubes
vip
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Tubes with complex shapes
Dezer
-
9 Years Ago
probably easier with prepreg and bladdermoulding... Do a quick search on google and you should find...
matthieutje65
-
9 Years Ago
I don't have any autoclave, it makes my job with prepreg difficult, and the cost of the part would...
Dezer
-
9 Years Ago
Does it matter if both inside and outside are smooth? If its the inside that younwant to keep smooth...
scottracing
-
9 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search