Dezer
Dezer
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 74,
Visits: 1.8K
Hi friends,
I would like to make a tube in the vacuum infusion process, but it has a complex shape, some tips or techniques how to do it?
Example:
Grateful for everyone's attention!!
Tags
pipes
tips
tubes
vip
Reply
Like
8
Matthieu Libeert
Matthieu Libeert
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
probably easier with prepreg and bladdermoulding...
Do a quick search on google and you should find what you need
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
8
Dezer
Dezer
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 74,
Visits: 1.8K
I don't have any autoclave, it makes my job with prepreg difficult, and the cost of the part would be more expensive as well.
matthieutje65
, thanks for your help.
Reply
Like
8
scottracing
scottracing
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
Does it matter if both inside and outside are smooth? If its the inside that younwant to keep smooth you may need to look into soluble mandrels.
Then get some braided material and infuse that. But as above to mkae tubes its much easier with prepreg. You can buy out of autoclave prepregs and cure them in a pid controlled oven
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search