Can anyone recommend a tack spray adhesive (preferably available in Australia) for use with Epoxy infusion. 3M Super 77 seems to get mentioned a lot but it sounds like it affectes the surface finish. Cytec Aerofix 3, from what I can determine, is intended for Polyester and Vinyl-ester resins, plus elite composites don't seem to be in business any more to supply it...

Thanks

Dave
Reply
SkiFreak
SkiFreak
Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)Supreme Being (203 reputation)
Group: Forum Members
Posts: 9, Visits: 122
I have just bought some tins of the 3M Super 77 spray adhesive and will do some testing to see if it works for me. If not I will need to go back to the Cytec Aerofix 3, but that is more than double the price, so I hope the 3M stuff works out.