Both the suggestions are good and may work. However you choose to try, the key thing is ensuring the material and bagging stack do not lift from the mould surface. I would favour a cut disc out of the cloth for this one, then overlap a second piece of cloth for the recess. There is less surface distortion of the main piece of cloth that way as you are not trying to force the cloth into a raised feature.The inside of the raised feature when demoulded is unlikely to be so visible that it matters if the weave on that piece has slight distortion.