CF wheelchair seat pan advice needed?


Author
Message
Dickie
Dickie
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 4, Visits: 14
Hi,
Currently I use 5.5mm non-structual interior grade hardwood plywood (from Wickes) for my wheelchair seat pan, it spans a distance of 350mm. On top of this I place my foam/memory foam cushion. The plywood gives me the right degree of rigidity/flexibility but adds more weight to my ultra-lightweight wheelchair than I would like. I would like to replace the plywood seat pan with carbon fibre or CF sandwich but don't know what type and thickness would give me a similar feel to 5.5mm plywood? I know some top-end wheelchair manufacturers give the option of carbon seat pans but I they're very rigid with little flex, especially for someone of my low weight. It doesn't have to one complete seat pan front to back, it can be slats.
NB: I weigh 53kg
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
A fine jigsaw blade will cut the foam core panel very easily.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search