Group: Forum Members
Posts: 592,
Visits: 1.9K
|
Sounds like you are not mixing correct ratio, or are working at way too low temperatures and/or high humidity..
I work in a small heated workshop, that I keep at 20 degrees C. I've never had any issues with XCR -- in fact it is by far the best skinning and coating epoxy I've ever worked with.
XCR seems to be very sensitive to getting the precise mixing ratio, so mixing very small batches can be tricky. I never mix less than 12 grams of resin to 4 grams of hardener.
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|