Hi guys I'm skinning a few parts and a issues I'm having now that hasn't happened before is the additional resin coats are lidying and flaking off.
Im using the xcr resin and adding the coats whilst the previous is still tacky,  also why does it go cloudy when it's wet sanded? 

Cheers 
By Interloper393 - 4/19/2017 11:53:52 AM

I do my skining in the house so always nice and warm buddy,  use the digital scales for ratio and mix for at least a few minutes. , first bunch of parts came out perfect and no issues, this is a new batch of resin and every part with it does this.