Interloper393
Interloper393
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 90,
Visits: 634
Hi guys I'm skinning a few parts and a issues I'm having now that hasn't happened before is the additional resin coats are lidying and flaking off.
Im using the xcr resin and adding the coats whilst the previous is still tacky, also why does it go cloudy when it's wet sanded?
Cheers
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Why is my resin peeling off?
Interloper393
-
9 Years Ago
Sounds like you are not mixing correct ratio, or are working at way too low temperatures and/or high...
Dravis
-
9 Years Ago
I do my skining in the house so always nice and warm buddy, use the digital scales for ratio and mix...
Interloper393
-
9 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search