Innegra


Author
Message
Junior
Junior
Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)
Group: Forum Members
Posts: 73, Visits: 473
Just wondered if anyone has ever used Innegra successfully to enhance the properties of their composite part, and where they have found it best placed within a laminate?

https://youtu.be/0N-LiWRA7RQ

Found the above video quite interesting but it defeats the object of having stiff Carbon by placing it on the outside?
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
I tried some pre preg innegra on some parts but I no longer trust using it.

It is basically a plastic which does not bond to the resins even though it talks of some surface treatment to assist bonding I have been able to simply pull the innegra skin apart from a carbon skin.

The material I used was also a tight weave and was far less conformable than a 200g twill carbon.




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search