Fasta
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
I tried some pre preg innegra on some parts but I no longer trust using it.
It is basically a plastic which does not bond to the resins even though it talks of some surface treatment to assist bonding I have been able to simply pull the innegra skin apart from a carbon skin.
The material I used was also a tight weave and was far less conformable than a 200g twill carbon.
Fastacraft Facebook page
Reply
Like
2
Junior
Junior
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 73,
Visits: 473
Just wondered if anyone has ever used Innegra successfully to enhance the properties of their composite part, and where they have found it best placed within a laminate?
https://youtu.be/0N-LiWRA7RQ
Found the above video quite interesting but it defeats the object of having stiff Carbon by placing it on the outside?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search