Talk Composites - The Forum for Advanced Composites

Innegra

http://www.talkcomposites.com/Topic23068.aspx

By Junior - 3/31/2017 8:14:46 PM

Just wondered if anyone has ever used Innegra successfully to enhance the properties of their composite part, and where they have found it best placed within a laminate?

https://youtu.be/0N-LiWRA7RQ

Found the above video quite interesting but it defeats the object of having stiff Carbon by placing it on the outside?
By Fasta - 4/1/2017 1:17:45 AM

I tried some pre preg innegra on some parts but I no longer trust using it.

It is basically a plastic which does not bond to the resins even though it talks of some surface treatment to assist bonding I have been able to simply pull the innegra skin apart from a carbon skin.

The material I used was also a tight weave and was far less conformable than a 200g twill carbon.