How much stronger is epoxy to polyester resin when using with Carbon/Kevlar and Fibreglass? It appears to be around double the price, but is double the strength?

People always recommend epoxy over polyester, but I notice that Polyester Resin is used a lot in boat making and boat repairs so surely it can't be that weak?
Reply
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
I've just found a paper written by SP Systems a few years ago and they suggest a 20-30% improvement in the mechanical properties of an Epoxy Resin over a Polyester Resin.