How much stronger is epoxy to polyester resin when using with Carbon/Kevlar and Fibreglass? It appears to be around double the price, but is double the strength?

People always recommend epoxy over polyester, but I notice that Polyester Resin is used a lot in boat making and boat repairs so surely it can't be that weak?
Replies
Junior
Junior
Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)
Group: Forum Members
Posts: 73, Visits: 473
Thanks for the informative answer! 

My thought process was in relation to kayak use (so not left in water for prolonged amounts of time). I'm trying to figure out the benefit of using Epoxy for the construction when it's twice the price. 

Does this mean kayaks made with epoxy have a polyester gel coat to protect the resin on the inside, or do they not suffer from hygroscopic problems due to not being kept in water?
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
yes, you could use a product such as our GC50 which is Polyester and thus acts to prevent the moisture absorption issue with Epoxy Resin but as you say, Kayaks are generally not kept in the water between uses and can dry out fully. Notwithstanding this, it would still be good practice to protect it with an exterior coating (either in-mould such as GC50 or post-mould such as Durepox) but most of the kayaks, especially competitive or adventure type will use epoxy for the enhanced strength characteristics.