How much stronger is epoxy to polyester resin when using with Carbon/Kevlar and Fibreglass? It appears to be around double the price, but is double the strength?

People always recommend epoxy over polyester, but I notice that Polyester Resin is used a lot in boat making and boat repairs so surely it can't be that weak?
Reply
Junior
Junior
Supreme Being (516 reputation)Supreme Being (516 reputation)Supreme Being (516 reputation)Supreme Being (516 reputation)Supreme Being (516 reputation)Supreme Being (516 reputation)Supreme Being (516 reputation)Supreme Being (516 reputation)Supreme Being (516 reputation)
Group: Forum Members
Posts: 73, Visits: 473
So if the exact same materials were layed up the same way, but one was laminated with general Epoxy resin and one with a similar Polyester Resin, how much mechanically stronger would the Epoxy lay up be?