Pattern coat system on ABS plastic


Author
Message
NMBROOK
NMBROOK
Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)Supreme Being (190 reputation)
Group: Forum Members
Posts: 4, Visits: 20
I am currently producing a plug to produce a fairly large multipiece mould for a model boat hull.The plug is an existing ABS plastic vac formed hull that has had alterations/additions in wood and bumper filler.The hull has been strengthened inside to increase rigidity to the necessary level.
My principle question is,can I safely use the pattern coat system over the top of this to get the desired finish?
I know I am safe with wood and the polyester based filler,but is the pattern coat system safe to use on Rigid ABS plastic?I do intend on using no finer than 120 grit prior to application in order to get a decent key.

Kind Regards

Nigel
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
In terms of coating the surface with a fresh layer of resin?  Yes certainly.  It can be a good way of both restoring a damaged boat hull at the same time as making it tidy enough to take a mould from.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Junior
Junior
Supreme Being (828 reputation)Supreme Being (828 reputation)Supreme Being (828 reputation)Supreme Being (828 reputation)Supreme Being (828 reputation)Supreme Being (828 reputation)Supreme Being (828 reputation)Supreme Being (828 reputation)Supreme Being (828 reputation)
Group: Forum Members
Posts: 73, Visits: 473
Warren (Staff) (28/03/2017)
In terms of coating the surface with a fresh layer of resin?  Yes certainly.  It can be a good way of both restoring a damaged boat hull at the same time as making it tidy enough to take a mould from.


Excellent! And it would bond to Polyethylene? 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
NMBROOK - 10 Years Ago
Hanaldo - 10 Years Ago
NMBROOK - 10 Years Ago
Hanaldo - 10 Years Ago
Matt (Staff) - 10 Years Ago
lino80 - 9 Years Ago
NMBROOK - 10 Years Ago
Warren (Staff) - 10 Years Ago
NMBROOK - 10 Years Ago
Junior - 9 Years Ago
Warren (Staff) - 9 Years Ago
Junior - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search