Id agree with bridging being a factor here. For vacuum bagging you want to ensure you are not using too high a level of vacuum as you may find you squeeze out too much resin. Typically you could be between 10-30% vacuum depending on the part.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|