Group: Administrators
Posts: 167,
Visits: 4.6K
|
Absolutely, for Infusion or PrePreg production, you always need to be running at full vacuum. For vacuum assisted wet lay, we find the best results are at lower vacuum levels as suggested above by Warren; the reason for this is that with too much resin, you ultimately draw more resin out of the part, through the release film and into the breather leaving you with low resin content and pin-holing or dry patches on the moulded face.
|