Hi I am making a canoe, for this I am manufacturing the mold and I would like to do it in two parts, separated by keel split mold, I can make vacuum infusion or these type of molds do not work with infusion.
0% - 0 votes
Member Votes: 0, Guest Votes: 0. This poll has been closed and is not accepting new votes
Author
Message
Grunge
Grunge
Supreme Being (220 reputation)Supreme Being (220 reputation)Supreme Being (220 reputation)Supreme Being (220 reputation)Supreme Being (220 reputation)Supreme Being (220 reputation)Supreme Being (220 reputation)Supreme Being (220 reputation)Supreme Being (220 reputation)
Group: Forum Members
Posts: 25, Visits: 178
Hi I am making a canoe, for this I am manufacturing the mold and I would like to do it in two parts, separated by keel split mold, I can make vacuum infusion or these type of molds do not work with infusion.
Edited 8 Years Ago by Warren (Staff)
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
If you were to use a gel coat then the finished part with come out of the mould with the split moulded into the new hull and sticking up slightly high. 

Then you just wet sand and polish the join and it should be invisible.