Lotus Exige Front Clam


Author
Message
MarkMK
MarkMK
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
No, quite a lot of cutting and jointing to get a decent weave alignment. Cutting templates made for the bonnet piece and some tricky cutting of the fabric whilst laying the main piece of fabric in the mould for the engine cover, after the small vertical pieces had been laid in. 

240g fabric was used as it's more stable than 200g and is more drapable than something like Profinish. 
Biggerbigben
Biggerbigben
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 4, Visits: 107
Fair enough. Those parts look fantastic. Not sure my wide arch moulds are good enough in their current state to produce parts like those!
MarkMK
MarkMK
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Have you already made some moulds of various body sections? Post up some pics, as I'm sure that some imperfections can be made better or remedied in the final part. 
Biggerbigben
Biggerbigben
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 4, Visits: 107
Only have a few pics of my wide body..

http://img.photobucket.com/albums/v301/biggerbigben/24D82E3A-E0C8-4396-A7A5-72F7806BE781_zpsxqsprfvv.jpg


http://img.photobucket.com/albums/v301/biggerbigben/B15ECC6C-C163-400F-921D-00254FFE6AAD_zps0j2u51af.jpg


http://img.photobucket.com/albums/v301/biggerbigben/FA5A1E0E-E552-4636-A769-95E510B7BD6A_zpsxjclaeia.jpg





Hanaldo
Hanaldo
Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Sorry guys, I'm in Africa for the month so I have extremely limited internet access. Will fix the image links when I get home. 
MarkMK
MarkMK
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Did you produce those panels for your existing car or are they the ones you bought? I'm guessing that you've converted from an Elise body?

Am I correct in thinking that those rear quarter panels are specific to the conversion kit (I've made some of those also)
jdp530
jdp530
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 6, Visits: 69
MarkMK (02/02/2017)
As Hanaldo posted the pics up some time ago now, they've probably become unavailable feom the source. Some fine and meticulous work involved there, though

Not certain if the pics will load up okay from my phone, but I've recently made a couple of S1 bits too. They felt tricky enough, but nowhere near as much as a full clam
Biggerbigben
Biggerbigben
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 4, Visits: 107
MarkMK (09/02/2017)
Did you produce those panels for your existing car or are they the ones you bought? I'm guessing that you've converted from an Elise body?

Am I correct in thinking that those rear quarter panels are specific to the conversion kit (I've made some of those also)


No I made them. Have a look here.. http://www.edition38.com/forums/index.php?showtopic=499026&page=9 They are converted from an exige body. 

The first rear 3 piece clam moulds were a disaster as moulds stuck, so I redid them and now have a new set of moulds, certainly better just don't think they are good enough for carbon as still have mould imperfections so I might prep and spray up the car in undercoat as is then re-do moulds with flanges for vacuum bagging in mind etc. We'll see as a lot of work! 

Only pic of 2nd rear clam mould I have to hand -

http://img.photobucket.com/albums/v301/biggerbigben/02E7CE35-0547-4D10-95E1-DD0582418B14_zpser7oij5e.jpg
MarkMK
MarkMK
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
Great work on those moulds and a shed load of effort and time spent I'm certain. Good to see that you've also managed to make it pay by selling on a set or two as well



Dan22h
Dan22h
Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)
Group: Forum Members
Posts: 15, Visits: 197
Seems to be a good few people making there own panels for these cars now. 
I'm working on this at the moment..



For this..


Edited 9 Years Ago by Dan22h