Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Aaaaaand because I'm now in a posting mood; the front bodywork I did for our Exige race car:
Wheel arches flared by 35mm:
Original fibreglass weight was 16kg. New carbon bodywork is 6kg, and infinitely stronger and stiffer.
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Lotus Exige Front Clam
Hanaldo
-
10 Years Ago
The spread tow racing stripe is sure getting popular :p Looking good I like the rings design...
davro
-
10 Years Ago
looking good, i know plenty of lotus owners in the uk that would love a front end like that!
scottracing
-
10 Years Ago
[quote][b]scottracing (16/04/2016)[/b][hr]looking good, i know plenty of lotus owners in the uk that...
Hanaldo
-
10 Years Ago
Looking good there Hanaldo, 6kg, tut tut, that's a bit heavy isn't it?? (only joking) How...
ChrisR
-
10 Years Ago
[quote][b]ChrisR (17/04/2016)[/b][hr]Looking good there Hanaldo, 6kg, tut tut, that's a bit heavy...
Hanaldo
-
10 Years Ago
Nice, there are a few places in the UK that do racing clams already but with mixed reviews. Some...
ChrisR
-
10 Years Ago
[quote][b]Hanaldo (16/04/2016)[/b][hr][quote][b]scottracing (16/04/2016)[/b][hr]looking good, i know...
scottracing
-
10 Years Ago
Very nice work!! I am equally impressed with how clean your floors are. Fred
fgayford
-
10 Years Ago
Nice work! I'm currently trying to build up my level of arsedness to do clams for the opel...
FLD
-
10 Years Ago
Brilliant! This is what we want to see! :) Was that sprayed with Sunshield?
Brian2fast
-
10 Years Ago
FLD, no, this mould is far too big for envelope bagging. I could have made it work by joining...
Hanaldo
-
10 Years Ago
Fantastic work Hanaldo That mould looks great and Ive no doubt that a great deal of thought went...
MarkMK
-
10 Years Ago
The greatest challenge was definitely laying up the mould. Not sure if you guys in the Northern...
Hanaldo
-
10 Years Ago
Hanaldo I'm guessing from your lay-up method that it wasn't possible to apply any sort of in-mould...
MarkMK
-
10 Years Ago
Mark, It's certainly would have been possible to use an in-mould coating. The main reason I didn't...
Hanaldo
-
10 Years Ago
Images don't seem to be working in the first post.. any chance these can be sorted as would love to...
Biggerbigben
-
9 Years Ago
As Hanaldo posted the pics up some time ago now, they've probably become unavailable feom the...
MarkMK
-
9 Years Ago
[quote][b]MarkMK (02/02/2017)[/b][hr]As Hanaldo posted the pics up some time ago now, they've...
jdp530
-
9 Years Ago
Those parts look good Mark, did you make them with one piece of cloth (without any joins)?
ChrisP
-
9 Years Ago
No, quite a lot of cutting and jointing to get a decent weave alignment. Cutting templates made for...
MarkMK
-
9 Years Ago
Fair enough. Those parts look fantastic. Not sure my wide arch moulds are good enough in their...
Biggerbigben
-
9 Years Ago
Have you already made some moulds of various body sections? Post up some pics, as I'm sure that some...
MarkMK
-
9 Years Ago
Only have a few pics of my wide body..
Biggerbigben
-
9 Years Ago
Sorry guys, I'm in Africa for the month so I have extremely limited internet access. Will fix the...
Hanaldo
-
9 Years Ago
Did you produce those panels for your existing car or are they the ones you bought? I'm guessing...
MarkMK
-
9 Years Ago
[quote][b]MarkMK (09/02/2017)[/b][hr]Did you produce those panels for your existing car or are they...
Biggerbigben
-
9 Years Ago
Great work on those moulds and a shed load of effort and time spent I'm certain. Good to see that...
MarkMK
-
9 Years Ago
Seems to be a good few people making there own panels for these cars now. I'm working on this at the...
Dan22h
-
9 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search