Lotus Exige Front Clam


Author
Message
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Aaaaaand because I'm now in a posting mood; the front bodywork I did for our Exige race car:

https://scontent.fper1-1.fna.fbcdn.net/hphotos-xpt1/v/t1.0-9/12510464_754090401389045_1014295541450088279_n.jpg?oh=581f8960a8f4aed7c19db3132de06fde&oe=57B2D702








Wheel arches flared by 35mm:

https://scontent.fper1-1.fna.fbcdn.net/hphotos-xpt1/v/t1.0-9/12400969_754090434722375_6186128354710743509_n.jpg?oh=5302dc5b86739ed0e2503098c92c5bb4&oe=57BC045D


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xap1/v/t1.0-9/12509509_754090464722372_2092220812819363509_n.jpg?oh=96343179a398bf958dad7875fe29a668&oe=5779BE98


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xal1/v/t1.0-9/21597_754090551389030_4208215315092582167_n.jpg?oh=58c6d9c91c4d0272e349e353304620bf&oe=57735224


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xal1/v/t1.0-9/12509060_755197027945049_935454048942021816_n.jpg?oh=ff8d320e795e954649ff47b858600f1c&oe=57727C62


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xfp1/v/t1.0-9/12410580_756027927861959_6215363780583939522_n.jpg?oh=49dbf5ca59486f393ad427e92b4e8de6&oe=577EF8B7


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xfa1/v/t1.0-9/12376390_756028047861947_3998638707266294953_n.jpg?oh=eab92c04ce64190ed1d0b2bef70bcfaa&oe=577863C3


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xpt1/v/t1.0-9/12645168_761150697349682_1168022580728239627_n.jpg?oh=68057e34ef3f4c66e519eabfa0dcc98a&oe=578006D6


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xpt1/v/t1.0-9/12642454_761150747349677_8631496522627503661_n.jpg?oh=0b8b976a70af79ad636f793d41458127&oe=577AF4A1


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xal1/v/t1.0-9/10436170_785219404942811_4162536039715637739_n.jpg?oh=097264ec1b98e1970da1e809f79379cf&oe=577B76BE


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xlp1/v/t1.0-9/943852_786486901482728_8871403028792424093_n.jpg?oh=b5ceb99e3fe6e53f82b1aa62a8a11adb&oe=57B5C05D


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xaf1/v/t1.0-9/10288767_786486914816060_5653877130849892348_n.jpg?oh=d319bb775dcfe27b9811b2cf1974dd01&oe=577D50D2


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xpl1/v/t1.0-9/10583841_786487001482718_4358172456970746280_n.jpg?oh=2a4cb0222021fb0431be7b6637642a70&oe=57B41FD6


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xpf1/v/t1.0-9/12006174_787969344667817_1056262774617378008_n.jpg?oh=cf60f06c797e661594e181e19e83d41c&oe=57BBE3A2








Original fibreglass weight was 16kg. New carbon bodywork is 6kg, and infinitely stronger and stiffer.
Replies
Biggerbigben
Biggerbigben
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 4, Visits: 107
Images don't seem to be working in the first post.. any chance these can be sorted as would love to see your exige. Have a wide body s1 myself and I'm thinking of going CF body!
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
As Hanaldo posted the pics up some time ago now, they've probably become unavailable feom the source. Some fine and meticulous work involved there, though

Not certain if the pics will load up okay from my phone, but I've recently made a couple of S1 bits too. They felt tricky enough, but nowhere near as much as a full clam
jdp530
jdp530
Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)
Group: Forum Members
Posts: 6, Visits: 69
MarkMK (02/02/2017)
As Hanaldo posted the pics up some time ago now, they've probably become unavailable feom the source. Some fine and meticulous work involved there, though

Not certain if the pics will load up okay from my phone, but I've recently made a couple of S1 bits too. They felt tricky enough, but nowhere near as much as a full clam
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Hanaldo - 9 Years Ago
davro - 9 Years Ago
scottracing - 9 Years Ago
Hanaldo - 9 Years Ago
ChrisR - 9 Years Ago
Hanaldo - 9 Years Ago
ChrisR - 9 Years Ago
scottracing - 9 Years Ago
fgayford - 9 Years Ago
FLD - 9 Years Ago
Brian2fast - 9 Years Ago
Hanaldo - 9 Years Ago
MarkMK - 9 Years Ago
Hanaldo - 9 Years Ago
MarkMK - 9 Years Ago
Hanaldo - 9 Years Ago
Biggerbigben - 8 Years Ago
MarkMK - 8 Years Ago
jdp530 - 8 Years Ago
ChrisP - 8 Years Ago
MarkMK - 8 Years Ago
Biggerbigben - 8 Years Ago
MarkMK - 8 Years Ago
Biggerbigben - 8 Years Ago
Hanaldo - 8 Years Ago
MarkMK - 8 Years Ago
Biggerbigben - 8 Years Ago
MarkMK - 8 Years Ago
Dan22h - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search