Aprilia MXV 450 : Motocross full carbon project completed.


Author
Message
Thanasis
Thanasis
Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)
Group: Forum Members
Posts: 36, Visits: 234
After 1 year, many hours of work, 16 moulds, some carbon parts born for scrap, some of them with very short riding life, some sticking conditions from moulds to parts and vise versa, I finished my motocross carbon project!

From plastic:
http://www.talkcomposites.com/Uploads/Images/838f6136-3f83-44aa-8814-1489.jpg


To carbon:
http://www.talkcomposites.com/Uploads/Images/65e5ac0e-1de4-4f78-be22-0c27.jpg


The loss of weight was not the main issue, the main goal of project was to make the rear fender stop cracking while riding in heavy mud and specially with supsension bottoming on bigger jumps. In muddy conditions the rear fender was bound to broke damaging also the rear side panels.
Making just the rear fender in carbon didn't help very much the situation. Final solution achieved by making the three seperate plastic parts (rear mudgard and the two side panels) just in one piece. A three piece mould was needed for this purpose:
http://www.talkcomposites.com/Uploads/Images/5b26b33a-5f52-4f54-a93e-c6dd.jpg

Unfortunately the first mould produced a slightly wrong dimensioned part (with a lot of aesthetic problems also). The one piece tail could not fit correctly in the subframe. Both mould and part go straight to trash. Starting from scratch the mould, this time the 3 plastic parts were tighten in the subframe and the mould was produced with all of them sitting in the right position.
The mk.1 part was good enough but not perfect. it last a lot of motocross riding hours but failed a little bit in very heavy mud. It was the time for mk.2 rear fender, this time more stiffer and 100 grams more heavier than mk.1.
Mk.2 turned to be perfect and very good looking.
http://www.talkcomposites.com/Uploads/Images/e35f5d8f-9a3e-4361-bfd8-ff57.jpg  
http://www.talkcomposites.com/Uploads/Images/a2b3873c-8d40-44d9-af11-bfa9.jpg


http://www.talkcomposites.com/Uploads/Images/2824a3ff-e2b4-470b-9d82-51a9.jpg


http://www.talkcomposites.com/Uploads/Images/60f9e3e7-4673-44f2-8c78-a019.jpg


http://www.talkcomposites.com/Uploads/Images/fd9ed53b-a57e-47f5-bab5-1d5a.jpg


It is tested in the mudiest conditions with success!

The fever of carbon modification was all over me and the rest of the parts were mend to be carbon also....
Edited 10 Years Ago by Izo78
Reply
Thanasis
Thanasis
Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)Supreme Being (592 reputation)
Group: Forum Members
Posts: 36, Visits: 234
So I found finally some time to finish the mould. It is ready to go!

http://www.talkcomposites.com/Uploads/Images/269f0443-34da-43d3-b14f-5924.jpg 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Izo78 - 10 Years Ago
Izo78 - 10 Years Ago
Izo78 - 10 Years Ago
Izo78 - 10 Years Ago
scottracing - 10 Years Ago
Izo78 - 10 Years Ago
Julien - 10 Years Ago
Izo78 - 10 Years Ago
hayeglas - 10 Years Ago
Izo78 - 10 Years Ago
morepower - 10 Years Ago
Izo78 - 10 Years Ago
Dravis - 10 Years Ago
Izo78 - 10 Years Ago
davro - 10 Years Ago
Thomb - 10 Years Ago
Izo78 - 10 Years Ago
Izo78 - 9 Years Ago
Thomb - 9 Years Ago
Izo78 - 9 Years Ago
     How it's going.
Shaneer22 - 9 Years Ago
Izo78 - 9 Years Ago
                 please make some pics! always nice to see.
Thomb - 9 Years Ago
Izo78 - 9 Years Ago
                         Well done mate, really looks nice :)
Thomb - 9 Years Ago
Warren (Staff) - 9 Years Ago
Izo78 - 9 Years Ago
Izo78 - 9 Years Ago
Hanaldo - 9 Years Ago
Izo78 - 9 Years Ago
Thomb - 9 Years Ago
Izo78 - 9 Years Ago
Izo78 - 9 Years Ago
Izo78 - 9 Years Ago
Rich (Staff) - 9 Years Ago
     nice work!!
Thomb - 9 Years Ago
Izo78 - 9 Years Ago
Warren (Staff) - 9 Years Ago
Izo78 - 9 Years Ago
Thomb - 9 Years Ago
Izo78 - 9 Years Ago
ThomPa - 9 Years Ago
Izo78 - 9 Years Ago
Izo78 - 7 Years Ago
Hanaldo - 7 Years Ago
Izo78 - 7 Years Ago
FRTCARBON - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search