Hi Shaz,
Yes you can use wet sanding during Step 12. Normally it is not necessary as the sanding at 240 grit will in most cases take out the dry 120 grit scratches. But there is no harm in wet sanding at 120 Grit.
For the lumpy edges, now is the time to shape and flatten them with the sandpaper. keep at the 120grit until you get it flat and to the desired shape. If you are going through to the carbon, stop, thoroughly clean the part, then re-coat in XCR so you have enough resin to sand to the desired shape.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|