regarding the 4 mounting points for the frame mounting, I would have some machined, in a shape that distributes the load out onto the flat sides you are adding to the frame in Carbon. Consider welding alu- "eyelets" on to flat pieces of aluminium ..
Also, I would certainly make this as a sandwich with either Soric or 3D core -- You can then "overengineer" without adding too much unneeded weight -
I would also consider adding at least one layer of Kevlar /CF mix cloth in the "stack" Just to make sure of keeping even a broken subframe mostly in one piece