R/c Spoiler


Author
Message
James91h
James91h
Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)
Group: Forum Members
Posts: 20, Visits: 217
Hi all,

Just wanted to hear your methods and thoughts.

For my next project I am making a spoiler for a remote controlled car, which is a fairly simple curved design much like an F1 wing minus the side plates.

I am looking for a perfect cosmetic finish so I was intending on doing a resin infusion, however I would like a gloss finish on both sides of the part.

I have read about doing the infusion without peel ply and using a core material for flow media then just using vacuum bagging straight over the carbon fabric but this still wont give a perfect finish..




What are my options other than making two halves and gluing together?




Thanks in advance!
Reply
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
How thick will the final piece be and the dimensions of the part?

Sounds like a matched mould would work in the situation, giving A side finish both sides, if it's thin i.e. a few plys then you could probably infuse without media using a very low viscosity resin.

I'd be tempted to wet lay and compress with a top mould before messing around with infusion 