Epoxy resin instead of CG50


Author
Message
Almand
Almand
Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)Supreme Being (254 reputation)
Group: Forum Members
Posts: 19, Visits: 108
I have made my first part using CG50 gelcoat, but it delamimate, so I wonder if it´s possible to spray epoxy resin in the mould instead off CG50, let it cure till it´s tacky, add reinforcement and then infuse?

Best regards

Keld
Edited 10 Years Ago by Almand
Reply
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
I don't use any gelcoat when infusing, lay up dry into the mould, infuse, then just spray on a UV topcoat after
Edited 10 Years Ago by ChrisR
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search