By Almand - 11/22/2016 9:09:42 AM
I have made my first part using CG50 gelcoat, but it delamimate, so I wonder if it´s possible to spray epoxy resin in the mould instead off CG50, let it cure till it´s tacky, add reinforcement and then infuse?
Best regards
Keld
|
By Almand - 12/6/2016 11:36:59 AM
Hi Hanado, thanks for reply...
No we used a expoxy resin from DK, perhaps we should try Easy composites. Or just sand well 
best regards
Keld
|
|