Owen
Owen
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 53
Hi there just want a little advice.
I want to glue 30mm x 400mm x 1.5mm strips of Nylon to steel box section (painted with 2k satin black) to act as non friction layer between this frame and a further piece of steel.I want to ask what adhesive would be best, Epoxy like ET515, Polyurethane like PT326 or something else? The steel is mounted to the back of a 4x4 truck as a bike rack and therefore is exposed to the elements.
Thanks!
Owen
Reply
Like
4
Reply
Owen
Owen
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 53
Specialist adhesive for Nylon being what?
Where if not from you would I get such an adhesive?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Nylon to steel
Owen
-
9 Years Ago
Hi Owen, Nylon is one of the hard to bond to plastics due to being very inert. Ideally we would...
Warren (Staff)
-
9 Years Ago
Specialist adhesive for Nylon being what? Where if not from you would I get such an adhesive?
Owen
-
9 Years Ago
You might have better success with a 3m VHB tape. Many of the 59 series tapes are recommended for...
nc42
-
9 Years Ago
It is not a product we stock. Your best bet is to try various adhesive manufacturers to see if they...
Warren (Staff)
-
9 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search