I want to glue 30mm x 400mm x 1.5mm strips of Nylon to steel box section (painted with 2k satin black) to act as non friction layer between this frame and a further piece of steel.I want to ask what adhesive would be best, Epoxy like ET515, Polyurethane like PT326 or something else? The steel is mounted to the back of a 4x4 truck as a bike rack and therefore is exposed to the elements.